Tanks and membranesExplainer

Fixing the membrane to the tank wall: rails, straps, perimeter sealing and welds

The membrane fixing at the top of the wall is one of the most heavily loaded points of the cover. We explain how rails, straps and welds work and what to inspect.

Published 5 min readFeedstockData Editorial Team

Other language versions: Polski, Deutsch, Español, Français, Italiano, Nederlands.

Biała kopuła membranowa fermentora nad ciemnozielonym zbiornikiem, z okrągłymi wziernikami.
Photo AxelHirsch / Wikimedia Commons, licence CC BY-SA 4.0, source file; changes: cropping

A tank membrane is only as tight as its weakest joint, and the weakest joints are usually found along the perimeter, in the corners and at pipe penetrations. The film or coated fabric itself has a large strength reserve, but the place where it passes into the rigid concrete or steel structure is subject to concentrated stresses, moisture and corrosion. This article explains how the perimeter fixing is built, how the methods of joining sheets differ and which symptoms indicate progressive weakening.

How the membrane is held on the wall

In a typical solution the membrane (one or two layers) is led over the top of the wall and clamped. Three basic arrangements are found:

Arrangement Principle Strengths Weaknesses
Clamping rail with gasket a flat rail presses the membrane against the top of the wall on anchors even pressure, possibility of re-tightening corrosion of anchors and bolts, loosening
Profile with a cord (rope) in a pocket the membrane edge has a welded pocket containing a cord clamped in a profile no point puncturing of the membrane requires precise routing, risk of slipping out
Fixing strap with anchors a strap bolted to the wall, the membrane welded or clamped on the strap easy installation more puncture points, more places of potential leakage

We compare the types of roofs in the article on the single- and double-membrane roof, and the loads from wind and snow in the text on wind, snow and ice. Whatever the arrangement, tightness is decided by a third layer that cannot be seen from outside, namely the surface of the top of the wall. Unevenness, sharp concrete edges or leftover formwork cause local abrasion. For this reason the surface is prepared so that it is level and free of sharp edges, and protective layers and gaskets of suitable hardness are used at the contact points.

Welds versus gluing

Membrane sheets are joined by welding or gluing, depending on the material. In practice two welding methods dominate: hot air or wedge and high frequency (HF). A correctly made weld creates a joint with a strength close to that of the base material, whereas gluing is used for repairs and for sealing details, because its quality is slower to check.

Weld quality depends on several parameters that the operator should also know, because they determine the warranty and durability:

  • cleanliness and dryness of the surface, free of moisture, grease and dust;
  • temperature, speed and pressure, matched to the material and the ambient temperature;
  • weld width and continuity check, e.g. an air-channel test or observation against the light;
  • sheet overlap arranged so that water runs over the overlap and not under it.

A perimeter weld in the cord pocket is particularly sensitive to delamination if the membrane works under high tension, e.g. with a full tank and strong wind.

Corners, creases and pipe penetrations

The membrane is meant to behave like a shell, so corners in the roof plan (e.g. in rectangular tanks or at channels) are difficult. Creases form where the material works in bending and becomes fatigued over filling cycles. Attention should be paid to places where permanent creases, whitening of the coating or blisters appear.

Pipe penetrations through the membrane are usually made as collars or stubs welded to the membrane. Their weak points are:

  1. the weld of the stub to the sheet, exposed to peeling when the pipe moves;
  2. clamping bands, which lose their pressure over time;
  3. corrosion of steel flanges in the atmosphere of humid biogas containing trace amounts of hydrogen sulphide.

Corrosion and loosening of connections

Fasteners work in a humid and aggressive atmosphere. Galvanised or stainless steel corrodes more slowly, but the zinc coating can be damaged during tightening. Temperature changes (the difference between winter and summer can exceed several dozen degrees) cause the membrane and bolts to expand and contract, and sealing materials show relaxation. As a result the pressure weakens. For this reason manufacturers usually recommend checking the tightening after the first season and then periodically; specific torques and intervals must always be taken from the instructions of the supplier of the given system.

What to inspect and when

The practical scope of inspecting the perimeter fixing can be limited to a few items:

  • a visual check of the whole perimeter for rust, cracked gaskets, loose bolts and bulges;
  • a spot check on a random sample to confirm that the fasteners have kept their pressure;
  • a leak check with a gas detector or a foaming solution, only under conditions consistent with safety rules and using equipment intended for explosion hazard zones;
  • a description and photograph of every defect in the register, to distinguish a progressive change from a one-off one.

A good time is spring, after the frosts have ended, and the period after strong storms. We describe methods of detecting leaks across the whole installation in the articles on the leak detection and repair programme and on optical gas imaging; what matters here is that the membrane perimeter is one of the places that must be inspected regularly, because its failure develops gradually and for a long time gives no symptoms in the operation of the cogeneration unit.

Let us remember that work on a membrane under gas pressure is work in an explosion hazard zone, and on the tank roof it is also work at height. Any repair work on the perimeter requires a procedure, non-sparking tools and the consent of the person responsible for the explosion protection document.

Sources

  1. FNR - Fachagentur Nachwachsende Rohstoffe (Leitfaden Biogas)
  2. KTBL - Biogas (Kuratorium für Technik und Bauwesen in der Landwirtschaft)